Are your bottles and jugs imploding? Add fluorine gas: fluoridated bottles

Do you recognize the problem of implosion as shown in the picture on the left? Are you still looking for a solution? Your partner in packaging can help.

The problem of bottles with dents is caused by volatile products that can migrate trough the HDPE side, which causes the bottle to contract.

Other occurring problems:

  • Alteration of the product
  • Loose labels on bottles and jerry cans
  • Slackening of the HDPE side
  • Etc.

Fluoridation is the clever way out for all these problems.
During the production of the HDPE packaging, fluorine gas is added, which causes the structure of the HDPE to change into a sort of teflon. All aforementioned problems can be solved this way. Don't hesitate to ask for the help your partner in packaging. We're ready if you are.